Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® A3HG6 WIT BK20560 - (PA66+PA6T/6)-(GF+GB)30 - BASF

Material Data Center offers the following functions for Ultramid® A3HG6 WIT BK20560:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Glass fibre reinforced injection moulding grade with good resistance to hydrolysis, suited for processing by water injection technology (WIT). Applications in the automotive cooling circuit, e.g. cooling water pipes.
Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 8 / * cm³/10min ISO 1133
온도 275 / * °C -
하중 5 / * kg -
성형 수축률, 평행 0.4 / * % ISO 294-4, 2577
성형 수축률, 수직 0.9 / * % ISO 294-4, 2577
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 8700 / 5300 MPa ISO 527
파단시 강도 165 / 95 MPa ISO 527
파단시 신율 3 / 4.9 % ISO 527
챠피 충격 강도 , +23°C 55 / 85 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 50 / 50 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 6 / 8 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 5 / 5 kJ/m² ISO 179/1eA
열적 특성건조/응축단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 230 / * °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 250 / * °C ISO 75-1/-2
기타 특성건조/응축단위시험규격
밀도 1370 / - kg/m³ ISO 1183
물질의 비성질건조/응축단위시험규격
ISO 데이터
점도수 146 / * cm³/g ISO 307, 1157, 1628
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 80 °C -
Pre-drying - Time 4 h -
Processing humidity ≤0.15 % -
용융수지온도 290 - 310 °C -
성형온도 80 - 90 °C -
도표
점도-변형률 , Ultramid® A3HG6 WIT BK20560, (PA66+PA6T/6)-(GF+GB)30, BASF
전단-변형률 , Ultramid® A3HG6 WIT BK20560, (PA66+PA6T/6)-(GF+GB)30, BASF
응력-신율 , Ultramid® A3HG6 WIT BK20560 (건조), (PA66+PA6T/6)-(GF+GB)30, BASF
응력-신율 , Ultramid® A3HG6 WIT BK20560 (응축), (PA66+PA6T/6)-(GF+GB)30, BASF
시컨트탄성율-신율 , Ultramid® A3HG6 WIT BK20560 (건조), (PA66+PA6T/6)-(GF+GB)30, BASF
시컨트탄성율-신율 , Ultramid® A3HG6 WIT BK20560 (응축), (PA66+PA6T/6)-(GF+GB)30, BASF
인장탄성율-온도 , Ultramid® A3HG6 WIT BK20560 (응축), (PA66+PA6T/6)-(GF+GB)30, BASF
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이), 검정
내화학성에
Hydrolytically Stable
응용
자동차의
지역별 검색
기타 정보
사E성
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 290 - 310 °C
injection molding, Melt temperature, recommended: 300 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
injection molding, Dwell time, thermoplastics: 10 min
화학적 매체에 대한 저항력
에서의 아세트산 (질량 5%) (23°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com